    Hello everyone,

    I am encountering a problem with the dispersion of styrene acrylate copolymer in a shower gel formula, and I need your help and technical advice to solve this problem. I am using the opacifier Empicol OP301 from HUNTSMAN in my formulation.

    I have conducted several tests by modifying the order of adding the opacifier (in the middle or at the end of the preparation) and varying the timing of its addition in relation to salt and fragrance to study their effects on the opacifier.

    Short-term stability tests (freeze/thaw) have revealed instability of the opacifier, which settles at the bottom of the bottle.

    I am facing a real blockage in solving this problem and would greatly appreciate your help.

    I also wonder if the quality of the opacifier (older production/recent production) might affect its stability.

    Thank you in advance.

    TYSS

    Original……….

    Bonjour à tous,

    Je rencontre un problème de dispersion du copolymère styrène acrylate dans une formule de gel douche et j’aurais besoin de votre aide et votre avis technique pour résoudre ce problème. J’utilise l’opacifiant Empicol OP301 de chez HUNSTMAN dans ma formulation.

    J’ai réalisé plusieurs essais en modifiant l’ordre d’ajout de l’opacifiant (au milieu ou à la fin de la préparation) et en variant le moment de l’ajout par rapport au sel et au parfum pour étudier leurs effets sur l’opacifiant.

    Les tests de stabilité à court terme (gel/dégel) ont révélé une instabilité de l’opacifiant, qui se retrouve au fond du flacon.

    Je suis confronté à un blocage réel pour résoudre ce problème et j’aimerais beaucoup votre aide.

    Je me demande également si la qualité de l’opacifiant (ancienne fabrication / fabrication récente) peut influencer sa stabilité.

    Merci d’avance

    TYSS

    Tyss replied 2 months, 1 week ago 4 Members · 6 Replies
  • 6 Replies
  • Adamnfineman

    Member
    May 10, 2024 at 10:22 am

    Bonjour!

    Peux-tu partager ta formule complète? Si non, peux-tu partager les autres ingrédients que t’utilize? Include les spécification de pH et viscosité stp.

    Ma première supposition est que tu n’as pas assez de viscosité pour suspendre ton opacifiant. Ma deuxième supposition est que ta formule a des électrolytes qui interfèrent avec la stabilité de votre opacifiant.

    English:

    Hello!

    Could you share your complete formula? If not, could you list the other ingredients used? Include the pH and viscosity please.

    My first guess is that you don’t have enough viscosity to suspend your opacifier. My second guess would be that your formula has electrolytes which interfere with your opacifier’s stability.

    • Tyss

      Member
      May 11, 2024 at 2:56 am

      Bonjour;

      Ma formule était la suivante:

      1- Aqua: QSP 100%

      2- Sodium laureth sulfate: 10%

      3- Sel fin marin: 1,4%

      4- EDTA 4 Na: 0,05%

      5- Huile d’olive: 0,02%

      6-PEG-40 hydrogenated castor: 0,15%

      7-Cocamidopropylbetaine 30%: 5%

      8-Coco glucoside: 1%

      9-Glycérine: 0,2%

      10-Cocamide DEA: 1,3%

      11-Acide citrique monohydrate: 0,04%

      12-Conservateur(MIT & MICT): 0,1%

      13-Parfum: 1,2%

      14-Colorant CI 16185: 0,002%

      Quant aux spécifications techniques du produit:

      * pH entre 5,5 et 6,5

      *Viscosité: entre 4500 et 7500 cP à 20°C

      Merci pour votre retour,

      Dans l’attente de votre feed back;

      Cordialement

      TYSS

      • Adamnfineman

        Member
        May 14, 2024 at 7:46 am

        Je suis d’accord avec @ketchito. Essaie sans le sel fin marin pour voir si c’est le problème.

        I agree with @ketchito. Try without the sel fin marin to see if it’s the problem.

  • ketchito

    Member
    May 13, 2024 at 6:30 am

    If sel fin marin is some sort of inorganic salt, then thatt might be the issue, since those opacifiers don’t get along with electrolytes. Try one batch without sel fim marin to confirm.

  • chemicalmatt

    Member
    May 14, 2024 at 3:19 pm

    As said by @ketchito You will find that acrylic disruption especially with divalent salts such as Mg, Ca as found in “l’eau marin”. Also, the acrylic opacifiers have ranges of pH compatibility and you must always add into water first before anything else, never last.

  • Tyss

    Member
    May 18, 2024 at 3:38 am

    <font style=”vertical-align: inherit;”><font style=”vertical-align: inherit;”>Bonjour;</font></font>

    <font style=”vertical-align: inherit;”><font style=”vertical-align: inherit;”><font style=”vertical-align: inherit;”><font style=”vertical-align: inherit;”>L’essai de ma formule de gel douche sans sel n’a pas été concluant. Un dépôt d’opacifiant se forme toujours au fond du flacon après 24 heures à 45°C, et cette fois-ci de manière notable. J’ai également effectué un autre essai avec sel, en utilisant un opacifiant d’un autre fournisseur (fiche technique en pièce jointe), mais j’observe toujours le même résultat : des petits points blancs au fond du flacon. Je me demande si la vitesse d’agitation et le temps de malaxage peuvent influencer la dispersion de l’opacifiant ou si le parfum pourrait en être la cause. Je vais essayer avec un échantillon sans parfum et un autre avec un parfum différent pour tester cette hypothèse.</font></font>
    </font></font>

    Je vous remercie tous pour cet échange qui m’a beaucoup aidé dans ma carrière professionnelle.

Log in to reply.