Face wash filling problem

Formula:
SLES , CAPB, COCODEA, Polyquat-7 & GHTC+Glycerin. 
I mix GHTc Paste after mixing all surfactant. 

Problem:
when filling into the tube, paste cut off improperly & fiber stick in side tube.
so after heat sealing end it leaks. Due to leakage high rejection.
Is serial of mixing GHTC paste ok?
or sholud i mix it first with SLES so that  it cut off properly.

GHTC 0.25% .
Without GHTC no rejection.
(sorry poor English)

Comments

  • WolfWolf Member
    The problem can be incorrect shut of time in the tube filling machine, or the fill nozzle parts are worn and not seating correctly.

Sign In or Register to comment.